性能项目 | 试验条件[状态] | 测试方法 | 测试数据 |
比重 | | ASTMD792 | 1.17 | g/cm3 |
密度 | | ISO1183 | 1.17 | g/cm3 |
TensileModulus(1.91mm,CompressionMolded) | | ASTMD638 | 8.48 | MPa |
TensileModulus(1.91mm,CompressionMolded) | | ISO527-2 | 8.48 | MPa |
TensileStrength(Yield,1.91mm,CompressionMolded) | | ASTMD638 | 13.1 | MPa |
TensileStress(Yield,1.91mm,CompressionMolded) | | ISO527-2 | 13.1 | MPa |
TensileElongation(Break,1.91mm,CompressionMolded) | | ASTMD638 | 300 | % |
TensileStrain(Break,1.91mm,CompressionMolded) | | ISO527-2 | 300 | % |
弹性体 | | TestMethod | NominalValue | Unit |
拉伸永久变形 | | ASTMD412 | 24 | % |
TearStrength2(24°C) | | ASTMD624 | 62.2 | kN/m |
DurometerHardness(ShoreA,1.91mm,CompressionMolded) | | ASTMD2240 | 93 | |
IRHD硬度 | | ISO48 | 93 | |
体积变化 | 24°C,168hr,inReferenceFuelB | ASTMD471 | 43 | % |
体积变化 | 100°C,168hr,inASTM#1Oil | ASTMD471 | -10 | % |
体积变化 | 100°C,168hr,inASTM#3Oil | ASTMD471 | 31 | % |