性能项目 | 试验条件[状态] | 测试方法 | 测试数据 |
比重2 | | ASTMD792 | 1.02 | g/cm3 |
抗张强度 | | ASTMD412 | 13.8 | MPa |
伸长率(断裂) | | ASTMD412 | 300 | % |
ChangeinRelativePermittivity | 1-14days | UL44 | 1.0 | % |
ChangeinRelativePermittivity | 7-14days | UL44 | -3.0 | % |
拉伸强度保持率-7days(121°C) | | ASTMD412 | 80 | % |
伸长保持率-7days(121°C) | | ASTMD412 | 80 | % |
热变形(131°C) | | UL44 | <15 | % |
热固性-Elongation3(200°C) | | IEC60811-2-1 | <50 | % |
相对电容率4 | | UL44 | 4.00 | |
Capacitance5 | pf,1day:90°C | UL44 | 950 | |
Capacitance5 | pf,14days:90°C | UL44 | 950 | |
Capacitance5 | pf,7days:90°C | UL44 | 950 | |
极限氧指数 | | ASTMD2863 | 26 | % |
火焰试验-Horizontal,No.4AWG60milwall6 | | UL44 | Pass | |
CrushingTest | | UL44 | 5605 | N |
Flexibility-4hrs6(-25°C) | | UL854 | Novisiblecracks | |