性能项目 | 试验条件[状态] | 测试方法 | 测试数据 |
比重1 | | ASTMD792 | 0.940 | g/cm3 |
熔流率(熔体流动速率)(190°C/2.16kg) | | ASTMD1238 | 2.9 | g/10min |
抗张强度2(屈服,滚塑成形) | | ASTMD638 | 17.9 | MPa |
伸长率3(断裂,滚塑成形) | | ASTMD638 | 400 | % |
弯曲模量-1%正割(滚塑成形) | | ASTMD790 | 848 | MPa |
ImpactStrength(-40°C,3.18mm,滚塑成形) | | ARM | 85 | J |
载荷下热变形温度(0.45MPa,未退火,滚塑成形) | | ASTMD648 | 61.0 | °C |