性能项目 | 试验条件[状态] | 测试方法 | 测试数据 |
熔流率(熔体流动速率)(190°C/2.16kg) | | ISO1133 | 15 | g/10min |
拉伸模量 | | ISO527-2 | 3200 | MPa |
拉伸应力(屈服) | | ISO527-2 | 67.0 | MPa |
拉伸应变(屈服) | | ISO527-2 | 13 | % |
标称拉伸断裂应变 | | ISO527-2 | 18 | % |
弯曲模量 | | ISO178 | 2900 | MPa |
简支梁缺口冲击强度 | -30°C | ISO179/1eA | 8.0 | kJ/m2 |
简支梁缺口冲击强度 | 23°C | ISO179/1eA | 9.0 | kJ/m2 |
热变形温度(0.45MPa,未退火) | | ISO75-2/B | 160 | °C |
热变形温度(1.8MPa,未退火) | | ISO75-2/A | 90.0 | °C |
熔融温度2 | | ISO11357-3 | 178 | °C |
AnnealingTemperature | | | 160 | °C |
AnnealingTime-Optional | | | 30.0 | min/mm |
漏电起痕指数 | | IEC60112 | 600 | V |
BurningRate3(1.00mm) | | ISO3795 | <100 | mm/min |
UL阻燃等级 | 0.75mm | UL94 | HB | |
UL阻燃等级 | 1.5mm | UL94 | HB | |
FlammabilityClassification | 0.75mm | IEC60695-11-10,-20 | HB | |
FlammabilityClassification | 1.5mm | IEC60695-11-10,-20 | HB | |
FMVSS可燃性 | | FMVSS302 | B | |
补充信息 | | TestMethod | NominalValue | Unit |
Emission | | VDA275 | <8.00 | mg/kg |
EmissionofOrganicCompounds | | VDA277 | 6.00 | ugC/g |