性能项目 | 试验条件[状态] | 测试方法 | 测试数据 |
熔流率(熔体流动速率)(190°C/2.16kg) | | ASTMD1238 | 2.5 | g/10min |
醋酸乙烯含量 | | ExxonMobilMethod | 12.0 | wt% |
拉伸模量2 | | ASTMD638 | 85.0 | MPa |
伸长率4(断裂) | | ASTMD638 | >100 | % |
SecantModulus-1%Secant,MD | | ASTMD882 | 78.0 | MPa |
SecantModulus-1%Secant,TD | | ASTMD882 | 83.0 | MPa |
抗张强度-MD(断裂) | | ASTMD882 | 30.4 | MPa |
抗张强度-TD(断裂) | | ASTMD882 | 27.8 | MPa |
伸长率-MD(断裂) | | ASTMD882 | 530 | % |
TensileElongation-TD(Break) | | ASTMD882 | 660 | % |
落锤冲击 | | ASTMD1709A | 480 | g |
埃尔曼多夫抗撕强度-MD | | ASTMD1922 | 110 | g |
ElmendorfTearStrength-TD | | ASTMD1922 | 160 | g |
肖氏硬度(邵氏A,15秒) | | ASTMD2240 | 94 | |
维卡软化温度 | | ASTMD1525 | 70.7 | °C |