性能项目 | 试验条件[状态] | 测试方法 | 测试数据 |
熔流率(熔体流动速率)(190°C/2.16kg) | | ASTMD1238 | 2.5 | g/10min |
SecantModulus-1%Secant,MD | | ASTMD882 | 1070 | MPa |
SecantModulus-1%Secant,TD | | ASTMD882 | 1500 | MPa |
抗张强度-MD(屈服) | | ASTMD882 | 32.1 | MPa |
TensileStrength-TD(Yield) | | ASTMD882 | 27.4 | MPa |
抗张强度-MD(断裂) | | ASTMD882 | 43.6 | MPa |
抗张强度-TD(断裂) | | ASTMD882 | 38.6 | MPa |
伸长率-MD(断裂) | | ASTMD882 | 790 | % |
TensileElongation-TD(Break) | | ASTMD882 | 6.0 | % |
落锤冲击 | | ASTMD1709 | 50 | g |
埃尔曼多夫抗撕强度-MD | | ASTMD1922 | 9.0 | g |
ElmendorfTearStrength-TD | | ASTMD1922 | 200 | g |