性能项目 | 试验条件[状态] | 测试方法 | 测试数据 |
密度 | | ASTMD1505 | 0.919 | g/cm3 |
熔流率(熔体流动速率)(190°C/2.16kg) | | ASTMD1238 | 1.0 | g/10min |
TensileStrength-MD(Break,30um,BlownFilm) | | ASTMD882 | 56.9 | MPa |
TensileStrength-TD(Break,30um,BlownFilm) | | ASTMD882 | 48.1 | MPa |
伸长率-MD(断裂,30um,吹塑薄膜) | | ASTMD882 | 480 | % |
TensileElongation-TD(Break,30um,BlownFilm) | | ASTMD882 | 620 | % |
落锤冲击(30um,吹塑薄膜) | | ASTMD1709A | 400 | g |
熔融峰值温度 | | ASTMD3418 | 107to117 | °C |
雾度(30.0um,吹塑薄膜) | | ASTMD1003 | 12 | % |