性能项目 | 试验条件[状态] | 测试方法 | 测试数据 |
密度 | | ASTMD1505 | 0.925 | g/cm3 |
熔流率(熔体流动速率)(190°C/2.16kg) | | ASTMD1238 | 0.80 | g/10min |
TensileStrength-MD(Break,50um,BlownFilm) | | ASTMD882 | 57.9 | MPa |
TensileStrength-TD(Break,50um,BlownFilm) | | ASTMD882 | 53.0 | MPa |
TensileElongation-MD(Break,50um,BlownFilm) | | ASTMD882 | 470 | % |
TensileElongation-TD(Break,50um,BlownFilm) | | ASTMD882 | 600 | % |
落锤冲击(50um,吹塑薄膜) | | ASTMD1709A | 350 | g |
熔融峰值温度 | | ASTMD3418 | 110to119 | °C |
雾度(50.0um,吹塑薄膜) | | ASTMD1003 | 12 | % |